Irreversible diameter change of wood segments correlates with other methods for estimating frost tolerance of living cells in freeze-thaw experiment: a case study with seven urban tree species in Helsinki - Archive ouverte HAL Accéder directement au contenu
Article Dans Une Revue Annals of Forest Science Année : 2015

Irreversible diameter change of wood segments correlates with other methods for estimating frost tolerance of living cells in freeze-thaw experiment: a case study with seven urban tree species in Helsinki

Anna Lintunen
  • Fonction : Auteur correspondant
  • PersonId : 1009436

Connectez-vous pour contacter l'auteur
Teemu Paljakka
  • Fonction : Auteur
  • PersonId : 1009437
Anu Riikonen
  • Fonction : Auteur
  • PersonId : 1009438
Leena Lindén
  • Fonction : Auteur
  • PersonId : 1009439
Lauri Lindfors
  • Fonction : Auteur
  • PersonId : 1009440
Eero Nikinmaa
  • Fonction : Auteur
  • PersonId : 1009441
Teemu Hölttä
  • Fonction : Auteur
  • PersonId : 888786

Résumé

AbstractKey messageWe assessed tree frost tolerance using electrolyte leakage and a method based on irreversible diameter change of branches. It was shown that irreversible diameter change correlates with electrolyte leakage and USDA hardiness rating and is a good indicator of frost tolerance.ContextThe number of potential tree species for urban green planning is low in northern latitudes where cold tolerance is a critical factor. High cost of urban tree establishment calls for reliable and preferably non-destructive methods for determining their cold tolerance.AimsWe studied the cellular damage occurring during freezing and thawing in branches of seven broadleaved tree species using electrolyte leakage and a method based on branch diameter changes.MethodsCellular damage in branches was studied during the cold-hardy stage in winter and the dehardening stage in early spring in laboratory conditions using both monitoring of frost-induced diameter changes and the common electrolyte leakage method during temperature decrease to −25 °C.ResultsFrost-induced irreversible diameter shrinkage correlated positively with electrolyte leakage. Out of the seven studied species, Quercus palustris and Crataegus monogyna had the highest frost tolerance during the dehardening stage in early spring, whereas Pterocarya fraxinifolia was the least frost tolerant.ConclusionIrreversible shrinkage of branch diameter due to freezing stress is a good and non-destructive method to indicate frost tolerance. It also correlates well with the USDA plant hardiness rating that is based on the minimum temperature range in which the studied species prevail in the USA.
Fichier principal
Vignette du fichier
13595_2015_Article_516.pdf (607.76 Ko) Télécharger le fichier
Origine : Publication financée par une institution
Loading...

Dates et versions

hal-01532272 , version 1 (02-06-2017)

Identifiants

Citer

Anna Lintunen, Teemu Paljakka, Anu Riikonen, Leena Lindén, Lauri Lindfors, et al.. Irreversible diameter change of wood segments correlates with other methods for estimating frost tolerance of living cells in freeze-thaw experiment: a case study with seven urban tree species in Helsinki. Annals of Forest Science, 2015, 72 (8), pp.1089-1098. ⟨10.1007/s13595-015-0516-3⟩. ⟨hal-01532272⟩
41 Consultations
67 Téléchargements

Altmetric

Partager

Gmail Facebook X LinkedIn More