Well-defined Phosphonated Homo- and Copolymers via Direct Ring Opening Metathesis Polymerization - Archive ouverte HAL Accéder directement au contenu
Article Dans Une Revue Polymer Année : 2013

Well-defined Phosphonated Homo- and Copolymers via Direct Ring Opening Metathesis Polymerization

Résumé

Phosphonated polymers with a well-defined molecular weight, composition, and architecture have been prepared via ring opening metathesis polymerization (ROMP) of diethyl phosphonate norbornene imides at room temperature for the first time. ROMP gave a broad range of phosphonated homopolymers, statistical, diblock and triblock copolymers based on poly(norbornene imide)s with low polydispersity (1.09-1.32) Complete hydrolysis of diethyl phosphonate poly(norbornene imide)s under mild conditions yielded the phosphonic acid derivatives. Thermogravimetric analysis indicated high thermal and thermo-oxidative stability of the polymers. Free standing and transparent films with good mechanical stability were obtained from the phosphonic acid functional homopolymers, diblock and triblock copolymers. Combining these basic properties with the advantages mentioned above make ROMP a promising pathway for accessing a wide diversity of phosphonated macromolecular structures. These new phosphonated polymers will open new perspectives in advanced application areas such as medicine and membrane science, which require a high level of control over polymer structure.

Domaines

Matériaux
Fichier principal
Vignette du fichier
Polymer13.pdf (1.24 Mo) Télécharger le fichier
Origine : Fichiers produits par l'(les) auteur(s)
Loading...

Dates et versions

hal-00904767 , version 1 (15-11-2013)

Identifiants

Citer

Bahar Bingöl, Anja Kroeger, Patric Jannasch. Well-defined Phosphonated Homo- and Copolymers via Direct Ring Opening Metathesis Polymerization. Polymer, 2013, pp.6676-6688. ⟨10.1016/j.polymer.2013.10.018⟩. ⟨hal-00904767⟩
142 Consultations
484 Téléchargements

Altmetric

Partager

Gmail Facebook X LinkedIn More