S. Wiederhorn, J. Lopez-cepero, and J. Wallace, Roughness of glass surfaces formed by sub-critical crack growth, Journal of Non-Crystalline Solids, vol.353, issue.16-17, pp.1582-1591, 2007.
DOI : 10.1016/j.jnoncrysol.2007.01.029

D. Hull, Fractography: observing, measuring, and interpreting fracture surface topography

G. Quinn, NIST recommended practice guide: fractography of ceramics and glasses, Special Publication (NIST SP), pp.960-916, 2006.
DOI : 10.6028/NBS.SP.960-16

J. Johnson and D. Holloway, On the shape and size of the fracture zones on glass fracture surfaces, Philosophical Magazine, vol.42, issue.130, pp.731-743, 1966.
DOI : 10.1080/14786445108561302

K. Ravi-chandar and W. Knauss, An experimental investigation into dynamic fracture: II. Microstructural aspects, International Journal of Fracture, vol.20, issue.1, pp.75-80, 1984.
DOI : 10.1007/BF01152313

J. Fineberg and M. Marder, Instability in dynamic fracture, Physics Reports, vol.313, issue.1-2, pp.1-108, 1999.
DOI : 10.1016/S0370-1573(98)00085-4

C. Wünsche, E. Rädlein, and D. Frischat, Glass fracture surfaces seen with an atomic force microscope, Fresenius J Anal Chem, vol.358, pp.349-351, 1997.

P. Gupta, D. Inniss, C. Kurkjian, and Q. Zhong, Nanoscale roughness of oxide glass surfaces, Journal of Non-Crystalline Solids, vol.262, issue.1-3, pp.200-206, 2000.
DOI : 10.1016/S0022-3093(99)00662-6

W. Raberg, A. Ostadrahimi, and T. Kayser, Atomic scale imaging of amorphous silicate glass surfaces by scanning force microscopy, Journal of Non-Crystalline Solids, vol.351, issue.12-13, pp.1089-1096, 2005.
DOI : 10.1016/j.jnoncrysol.2005.01.022

E. Bouchaud, Scaling properties of cracks, Journal of Physics: Condensed Matter, vol.9, issue.21, pp.4319-4344, 1997.
DOI : 10.1088/0953-8984/9/21/002

S. Wiederhorn, Influence of Water Vapor on Crack Propagation in Soda-Lime Glass, Journal of the American Ceramic Society, vol.42, issue.1, pp.407-414, 1967.
DOI : 10.1021/ja01168a005

F. Lechenault, C. Rountree, and F. Cousin, Evidence of Deep Water Penetration in Silica during Stress Corrosion Fracture, Physical Review Letters, vol.51, issue.16, 2011.
DOI : 10.1051/anphys:2008044

D. Marsh, Plastic Flow in Glass, Proceedings of the Royal Society A: Mathematical, Physical and Engineering Sciences, vol.279, issue.1378, pp.33-43, 1964.
DOI : 10.1098/rspa.1964.0114

M. Tomozawa, Fracture of Glasses, Annual Review of Materials Science, vol.26, issue.1, pp.43-74, 1996.
DOI : 10.1146/annurev.ms.26.080196.000355

S. Wiederhorn, T. Fett, and G. Rizzi, The effect of water penetration on crack growth in silica glass, Engineering Fracture Mechanics, vol.100, pp.3-16, 2013.
DOI : 10.1016/j.engfracmech.2012.04.026

URL : https://hal.archives-ouvertes.fr/hal-00830319

T. Fett, G. Rizzi, and D. Munz, T-stress solution for DCDC specimens, Engineering Fracture Mechanics, vol.72, issue.1, pp.145-149, 2005.
DOI : 10.1016/j.engfracmech.2004.03.006

M. He, M. Turner, and A. Evans, Analysis of the double cleavage drilled compression specimen for interface fracture energy measurements over a range of mode mixities, Acta Metallurgica et Materialia, vol.43, issue.9, pp.3453-3458, 1995.
DOI : 10.1016/0956-7151(95)00036-U

G. Pallares, L. Ponson, and A. Grimaldi, Crack opening profile in DCDC specimen, International Journal of Fracture, vol.89, issue.1???2, pp.11-13, 2009.
DOI : 10.1115/1.3601206

URL : https://hal.archives-ouvertes.fr/hal-00371380

G. Pallares, M. George, and L. Ponson, Abstract, Corrosion Reviews, vol.89, issue.6, pp.501-514, 2015.
DOI : 10.1209/0295-5075/89/66003

F. Lechenault, G. Pallares, and G. M. , Effects of Finite Probe Size on Self-Affine Roughness Measurements, Physical Review Letters, vol.104, issue.2, 2010.
DOI : 10.1088/0957-4484/4/2/006

URL : https://hal.archives-ouvertes.fr/hal-00534475

E. Bouchaud, The Morphology of Fracture Surfaces: A Tool for Understanding Crack Propagation in Complex Materials, Surface Review and Letters, vol.77, issue.05, pp.797-814, 2003.
DOI : 10.1103/PhysRevLett.90.075504

D. Bonamy, L. Ponson, and S. Prades, Scaling Exponents for Fracture Surfaces in Homogeneous Glass and Glassy Ceramics, Physical Review Letters, vol.703, issue.13, 2006.
DOI : 10.1103/PhysRevLett.87.187002

URL : http://arxiv.org/pdf/cond-mat/0608200

D. Dalmas, A. Lelarge, and D. Vandembroucq, Crack Propagation through Phase-Separated Glasses: Effect of the Characteristic Size of Disorder, Physical Review Letters, vol.56, issue.25, 2008.
DOI : 10.1016/S0997-7538(03)00078-0

URL : https://hal.archives-ouvertes.fr/hal-00201200

C. Kurkjian and W. Prindle, Perspectives on the History of Glass Composition, Journal of the American Ceramic Society, vol.15, issue.2, pp.795-813, 1998.
DOI : 10.1088/0022-3735/2/4/307

T. Fett, J. Guin, and S. Wiederhorn, Stresses in ion-exchange layers of soda-lime-silicate glass, Fatigue <html_ent glyph="@amp;" ascii="&"/> Fracture of Engineering Materials and Structures, vol.65, issue.6, pp.507-514, 2005.
DOI : 10.1111/j.1551-2916.2005.00108.x

F. Célarié, M. Ciccotti, and C. Marliere, Stress-enhanced ion diffusion at the vicinity of a crack tip as evidenced by atomic force microscopy in silicate glasses, Journal of Non-Crystalline Solids, vol.353, issue.1, p.51, 2007.
DOI : 10.1016/j.jnoncrysol.2006.09.034

S. Wiederhorn, T. Fett, and J. Guin, Griffith Cracks at the Nanoscale, International Journal of Applied Glass Science, vol.106, issue.10, pp.76-86, 2013.
DOI : 10.1103/PhysRevLett.106.165504

URL : https://hal.archives-ouvertes.fr/hal-01148305

H. Gao and J. Rice, Shear Stress Intensity Factors for a Planar Crack With Slightly Curved Front, Journal of Applied Mechanics, vol.53, issue.4, pp.774-778, 1986.
DOI : 10.1115/1.3171857

URL : http://esag.harvard.edu/rice/126_GaoRice_PerturbedCrackFront_JAM86.pdf

S. Ramanathan, D. Erta, and D. Fisher, Quasistatic Crack Propagation in Heterogeneous Media, Physical Review Letters, vol.76, issue.5
DOI : 10.1103/PhysRevLett.76.1087

URL : http://arxiv.org/pdf/cond-mat/9611196

F. Léonforte, A. Tanguy, and J. Wittmer, Inhomogeneous Elastic Response of Silica Glass, Physical Review Letters, vol.267, issue.5
DOI : 10.1103/PhysRevB.50.13105

M. Ciccotti, Stress-corrosion mechanisms in silicate glasses, Journal of Physics D: Applied Physics, vol.42, issue.21, 2009.
DOI : 10.1088/0022-3727/42/21/214006

URL : https://hal.archives-ouvertes.fr/hal-00354121

K. Han, M. Ciccotti, and S. Roux, Measuring nanoscale stress intensity factors with an atomic force microscope, EPL (Europhysics Letters), vol.89, issue.6, 2010.
DOI : 10.1209/0295-5075/89/66003

URL : https://hal.archives-ouvertes.fr/hal-00454092

J. Guin and S. Wiederhorn, Fracture of Silicate Glasses: Ductile or Brittle?, Physical Review Letters, vol.316, issue.21, 2004.
DOI : 10.1016/S0022-3093(02)01943-9

S. Wiederhorn, F. Yi, and D. Lavan, Volume Expansion Caused by Water Penetration into Silica Glass, Journal of the American Ceramic Society, vol.74, issue.10, pp.98-78, 2015.
DOI : 10.1111/j.1151-2916.1991.tb06801.x

M. Barlet, J. Delaye, and B. Boizot, From network depolymerization to stress corrosion cracking in sodium-borosilicate glasses: Effect of the chemical composition, Journal of Non-Crystalline Solids, vol.450, issue.450, pp.174-184
DOI : 10.1016/j.jnoncrysol.2016.07.017

URL : https://hal.archives-ouvertes.fr/cea-01483763

B. Warren, H. Krutter, and O. Morningstar, Fourier analysis of X-ray patterns of vitreous SiO

N. Bansal and R. Doremus, Handbook of Glass Properties, 1986.

M. Barlet, J. Delaye, and T. Charpentier, Hardness and toughness of sodium borosilicate glasses via Vickers's indentations, Journal of Non-Crystalline Solids, vol.417, issue.418, pp.417-418, 2015.
DOI : 10.1016/j.jnoncrysol.2015.02.005

C. Rountree, Recent progress to understand stress corrosion cracking in sodium borosilicate glasses: linking the chemical composition to structural, physical and fracture properties, Journal of Physics D: Applied Physics, vol.50, issue.34
DOI : 10.1088/1361-6463/aa7a8b

URL : https://hal.archives-ouvertes.fr/cea-01596241

A. Grimaldi, M. George, and G. Pallares, The Crack Tip: A Nanolab for Studying Confined Liquids, Physical Review Letters, vol.82, issue.16, 2008.
DOI : 10.1016/j.jnoncrysol.2006.09.034

URL : https://hal.archives-ouvertes.fr/hal-00411946