Effects of lux containing fluorides on TIG welding process

Résumé

The mechanisms of the inorganic powders, named activating flux and used in ATIG welding process, are not well identified. Oxides and fluorides usually compose activating fluxes. The present paper studies the fluoride activating effect. The analysis of the arc energy influence on the weld bead geometry allows determining the mechanisms that occur during ATIG welding with fluorides. Il seems that fluoride activating effect could depends on the fluoride lattice energy and/or the ionic radius of the element. Fluorides oct on the arc physics only. An arc energy densification is observed. Furthermore, an arc temperature increase, find out with optical emission spectrometry, characterises the fluoride activating effect. The fluorides do not affect the weld bead surface chemistry. Marangoni convection movements stay centrifugal as in TIG welding and do not favour e penetration increase.

Domaines

Matériaux
Fichier non déposé

Dates et versions

hal-00123072 , version 1 (08-01-2007)

Identifiants

Citer

S. Leconte, P. Paillard, P. Chapelle, G. Henrion, J. Saindrenan. Effects of lux containing fluorides on TIG welding process. Science and Technology of Welding and Joining, 2007, 12, n.2, pp.120-126. ⟨10.1179/174329307X159810⟩. ⟨hal-00123072⟩
44 Consultations
0 Téléchargements

Altmetric

Partager

Gmail Facebook X LinkedIn More