Résumé

To support optimisation of refractory masonry structures compressibility of dry joints of magnesia-carbon and magnesia-chromite bricks have been investigated. Laboratory scale tests and finite element modelling have been performed. Measurements done in wide temperature range have shown that the exponential form of the joint closure curve results from gradual closure of initially non-parallel surfaces. The stress needed to close the joint was found to be proportional to the material stiffness. Temperature influences the joint closure by changing the stiffness of material and by reducing the initial joint gap due to thermal expansion.
Fichier principal
Vignette du fichier
Compressive_behaviour_of_dry_joints_in_refractory_ceramic_masonry.pdf (697.64 Ko) Télécharger le fichier
Origine : Fichiers produits par l'(les) auteur(s)
Loading...

Dates et versions

hal-00772391 , version 1 (10-01-2013)

Identifiants

Citer

K. Andreev, Sido Sinnema, Amna Rekik, Samir Allaoui, Eric Blond, et al.. Compressive behaviour of dry joints in refractory ceramic masonry. Construction and Building Materials, 2012, 34, pp.402-408. ⟨10.1016/j.conbuildmat.2012.02.024⟩. ⟨hal-00772391⟩
95 Consultations
762 Téléchargements

Altmetric

Partager

Gmail Facebook X LinkedIn More